Cute Young Blonde Girl Near The Brick Wall
|
The soft mud method is the most common, as it is the most economical. It starts with the raw clay, preferably in a mix with 25-30% sand to reduce shrinkage. The clay is first ground and mixed with water to the desired consistency. The clay is then pressed into steel moulds with a hydraulic press. The shaped clay is then fired ("burned") at 900-1000 °C to achieve strength.
Rail kilns
In modern brickworks, this is usually done in a continuously fired tunnel kiln, in which the bricks move slowly through the kiln on conveyors, rails, or kiln cars to achieve consistency for all bricks. The bricks often have added lime, ash, and organic matter to speed the burning.
|
|